Evidence
316L Material Verification
316L is the default grade here and the only one we promote. Verification runs on two tracks. Incoming material is identified and stored by grade, and composition spot-checks cover finished parts. Mill test certificates depend on what the mill releases for each material, so not every order can carry one. Ask our sales team for which certificates can be prepared for your program.
Grade policy
One default grade, and a written exception
The largest fraud in this industry is grade substitution. The defense is a policy narrow enough to be audited, which is more than a promise.
| Grade | When it is used | How it is documented |
|---|---|---|
| 316L | Default for all customer programs and the only grade actively promoted | Stated on the specification sheet, verified against incoming certification and by spot-check |
| 304 | Only where a customer specifies it in writing | Grade named explicitly on the specification and the documentation, never abbreviated to just stainless steel |
| 201 | Only where a customer specifies it in writing | As above |
Claim boundary
What can legitimately be claimed about this material
Verification
How the grade is checked
Composition spot-checking is non-destructive, so it can run on finished parts rather than on a coupon that may or may not represent the batch.
| Sampling point | What is checked | Why here |
|---|---|---|
| Incoming material | Grade identification against the supplied certification | Catches a substitution before it enters a production run, when it is still cheap to fix |
| First article | Composition on the formed part, before the run proceeds | Confirms the material that reached the line, not the material on the paperwork |
| Findings and bought-in components | Composition on clasps, posts and jump rings | An otherwise correct piece can carry an unexpected grade in a bought-in component |
| Outgoing | Spot-check on finished goods | Last gate before the goods leave |
Incoming identification and segregated storage
Material is identified and stored by grade, with the separation physical rather than procedural. Labels alone do not prevent a mistake at the point of picking.
Record producedIncoming material record
First-article verification
The grade is confirmed on the first formed part before the run proceeds, alongside the dimensional first-article check.
Record producedFirst-article sheet
Outgoing spot-check
A final composition spot-check on finished goods, recorded against the batch.
Record producedOutgoing inspection report
Evidence
The records behind the grade
Mill test certificates
A mill test certificate ties the incoming material to a heat number at the mill, which is the deepest point ordinary verification reaches. It is also the document your importer will want for a different reason. Steel entered UFLPA high-priority enforcement in August 2025.
Raw material traceability and mill test certificatesFrequently asked questions
How do I know a piece is really 316L?
By composition, not by description. The two checkable routes are a mill test certificate tracing the incoming material to a heat number, and composition spot-checking on finished parts. Both are more useful than an invoice line, and both are things you can ask any supplier for. A supplier who can only offer the invoice line is not verifying anything.
Do you also make pieces in 304 or 201?
316L is the default and the grade we promote. 201 and 304 are supplied only where a customer specifies them in writing, and in that case the grade is disclosed on the documentation rather than being blurred into "stainless steel". We do not present ourselves as a multi-grade generalist, because in this industry that phrasing is usually where substitution starts.
Can stainless steel jewelry be described as corrosion-resistant?
For the base material, yes. 16 CFR §23.11(b) names austenitic stainless steels, which includes 304 and 316L, among the materials that support that claim. It is the strongest defensible claim available for this material in the US market. It applies to the steel, not to a coating sitting on top of it, and "resistant" is the ceiling. A stronger form, claiming the metal cannot corrode at all, would require it never to corrode anywhere under any conditions.
What stops grades getting mixed on the factory floor?
Three gates: incoming material identification and segregated storage, first-article verification before a run, and outgoing inspection.
Last updated